Old 06-09-2008, 10:59 AM
Jack Jack is offline
Moderator
 
Join Date: Jun 2002
Location: Georgia
Posts: 6,087
Westerner, welcome to Huntchat.
First, a question or two... how much of the case are you annealing, and what procedure do you use for annealing?
The thing I can think of off the top of my head is this: usually for blowing out cases in an improved chamber, the experts recommend using a medium charge of a medium speed powder, rather than the slower powder you'd normally load in an improved 243.
In other words, a middle of the range charge of a powder like 4895 rather than something slow like Reloder 22.
__________________
“May we never confuse honest dissent with disloyal subversion.”
Dwight D. Eisenhower
"If the freedom of speech is taken away, then dumb and silent we may be led, like sheep to the slaughter"
George Washington
Jack@huntchat.com
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 06:46 AM.


Powered by vBulletin® Version
Copyright ©2000 - 2013, Jelsoft Enterprises Ltd.